Effect of High-Energy Ball Milling on the Magnetic ...
S. Gao et al. 52 Figure 2. (a) The densities of the Ni 0.5Zn 0.5Fe 2O 4 ceramic samples prepared by SPS after high-energy ball milling for 20 h, 40 h, and 60 h (Dth = theoretical value); (b) The corresponding XRD patterns. milling …